PP Resemble Steel Fiber
Type: Other Fireproofing Materials | Place of Origin: Shandong China (Mainland) | Brand Name: DZLY | color: white,black |
PP Resemble-Steel-Fiber
PP Resemble Steel Fiber is a kind of substitute product of steel fiber, also has some specialties of the thin fiber. Compared with the steel fiber, it has the special features of anti corrosion,anti dispersion ,anti operation,no damage to the mixing equipment, etc This product is made of synthetic resin by special technique, has the advantages of high breaking tenacity, high-gripping force and excellent dispersivity in the concrete.
It can take place of steel fiber for the cement concrete, to improve the capability of crisp, the low tensile strength, the low elongation ultimate of the concrete instead of anti stretch, anti bending, anti fatigue, high tenacity and so on, so it got wide application in the construction,roads,bridges,hydraulic engineering and other engineering fields
The Physicochemical Properties of the Resemble-Steel-Fiber
Material Form | Polypropylene | Identical Diameter (mm) | 0.8±0.2(black);0.6±0.2(white) |
Color | black;white | Shape | waviness |
Length(mm) | 25±2(black);40±2(white) | Tensile Strength(MPa) | ≥500 |
The Function of Resemble-Steel-Fiber
1) Decrease the danger from crack of the concrete; increase the intensity of anti stretch, anti bending, anti breaking of the concrete
2) Decrease the breakage when earthquake or other terrible natural disasters happen
3) Decrease the inner fatal defect of the concrete; increase the anti infiltration performance of the concrete
4) Protect the steel bar from corroding; increase the durability of the concrete structure
5) Increase the abrasive resistance of the concrete
6) No abrasion to the mixing equipment
7) Prevent the damage to the tires
Compare with the Steel Fiber in Economy
Resemble Steel Fiber is made according to the function of the steel fiber. Its shape of cross section and specific
surface area are similar to the steel fiber, so when compare the economy of the two kind of material, we could
suppose that they have the same specific surface area and the proportion of the reinforced anti crack tendon is 0.95kg/cm3,
Packaging Detail:1.0kg inside plastic bag,11 bags in one woven bag,940 woven bags in one 40 FCL |
Delivery Detail:15~20 days after receive your advance payment |