Geosynthetic Clay Liner
GCLs (Geosythetic Clay Liners) are widely used in waste landfill and mining base seals, canal and dam liners, lakes and other wa - details see: https://www.buildingsupplieshub.com/geosynthetic-clay-liner-10100662
Type: Geosynthetic Clay Liner | Swell index: 24 ml/2g | | |
Mainfeatures of our company GCLs
a. Environment-preservation
b. Bentonite is one kind of water-proofing material processing of permanence and non-aging properties.
c. Installing facilitately.
d. Installing on the wet foundation directly.
e. Self-repair property
Installation Methods Disposal of sub grades 1. The sub grades must be tamped before paving the GCLs, the surface should be smooth. And it should not have the obvious hollow space. 2. The surface should be dry. 3. The minimum angle of land surface exposed to the sun should be more than 30cm. 4. The construction of GCLs should be begin until checking out the foundation Preparation before paving the GCLs - Drawing the GCLs paving order
- Examining the GCLs appearance quality
- The construction of GCLs should be processed under the weather with no rain and snow
GCLs paving - When paving the GCLs, it can use the machine and also the manpower.
- Paving the GCLs according to the stated order and way.
- Paving the GCLs, seaming overlapping between mat and mat should be staggered.
- There should not be sand and soil, hydrocele and so on impurity, to avoid affecting on the over lapping quality.
- To avoid the GCLs gliding, had best to fix it with nails when installing in vertical and
level. Such as drawing - Both sides of the GCLs are geotextile and woven geotextile, when paving, the geotextile should be nextto the water
- When paving, examine the GCLs appearance at any moment
Backfill - GCLs paved must be backfilled on the day.
- The sand or the sifted soil is the best choice, and the soil should not have impurity with
more than10mm. - The soil must be tamped every backfilling 50cm, and the degree of density should be more than 85%.
- Pay attention to the GCLs when tamping, it can not be damaged.
- When backfilling in the planar surface, the thickness should be 30cm at least.
|
Technical Specification MATERIAL PROPERTY | TEST METHOD | REQUIRE VALUES | Bentonite Swell Index | ASTM D 5890 | 24ml/2g min | Water Content(%) | ASTM D 4643 | 12 max | Bentonite Fluid Loss | ASTM D 5891 | 18ml max | Tensile Strength | ASTM D 4632 | 10.5KN min | Peel Strength | ASTM D 4632 | 65.8N min | Bentonite Mass/m2 | ASTM D 5084 | 5kg/ m2min | GCLs Permeability(flux index) | ASTM D 5887 | 5×10-8m3/m2.sec. | Vertically Osmotic Coefficient | ASTM D 5084 | 5×10-9m/s |
|
-